Active Standard
Most Recent

SAE AMS 5704L:2020-08-03

Nickel Alloy, Corrosion and Heat Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.6Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated

Summary

This specification covers a corrosion and heat-resistant nickel alloy in the form of forgings 3.25 inches (82.6 mm) and under, and forging stock of any size (see 8.6).

Technical characteristics

Publisher SAE International
Publication Date 08/03/2020
Page Count 7
Themes Aerospace
EAN ---
ISBN ---