€86.00
Titanium Bars, Wire, Forgings, and Rings Commercially Pure 70 ksi (483 MPa) Yield Strength
€81.00
Steel, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 17Cr - 13Ni - 2.5Mo (316L) Solution Heat Treated
€68.00
Steel, Bars, Forgings, and Tubing 1.2Cr - 3.2Ni - 0.12Mo (0.07 - 0.13C) (9310)
€71.00
Steel, Bars and Forgings 0.90Si 1.0Cr 2.0Ni 3.2Mo 2.0Cu 0.10V (0.07-0.13C) Vacuum Arc or Electroslag Remelted
€77.00
Steel Bars, Forgings, and Tubing 1.1Si - 1.45Cr - 1.0Mo - 0.08Al (0.16 – 0.22C) Double Vacuum Melted
Aluminum Alloy Bars, Rods, and Wire Rolled or Cold Finished, and Rings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T6, 7075-T651) Solution and Precipitation Heat Treated
Aluminum Alloy Bars, Rods, and Wire, Rolled or Cold Finished 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-F) As Fabricated, or when specified, Annealed (7075-O)
Aluminum Alloy, Hand Forgings 8.0Zn - 1.0Cu - 1.6Mg - 0.12Zr (7037-T7452) Solution Heat Treated, Compression Stress-Relieved, and Overaged
Standard Specification for Steel Investment Castings General Requirements, for Pressure-Containing Parts
This product is not for sale, please contact us for more information
Test Slabs, Acrylonitrile Butadiene (NBR-L) Low Acrylonitrile, 65 - 75
Aerospace series - Steel FE-PL1505 (15CrMoV6) - Air melted - Hardened and tempered - Bars - De = 16 mm - 980 MPa = Rm = 1 180 MPa
€50.00
Nickel Alloy, Corrosion and Heat-Resistant, Wire 74Ni - 15.5Cr - 8.0Fe Annealed
€70.00
Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta - 0.30Al - 0.05Zr - 0.05La - 0.20N Solution Heat Treated
Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength
€73.00