BS HR 10:1972

BS HR 10:1972

Superseded Historical

Specification for nickel-cobalt-chromium-molybdenum-titanium-aluminium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 20, Mo 5.9, Ti 2.1, Al 0.5)

€165.00

View more
BS HR 40:1972

BS HR 40:1972

Superseded Historical

Specification for cobalt-chromium-tungsten-nickel-manganese heat-resisting alloy billets, bars and forgings (cobalt base, Cr 20, W 15, Ni 10, Mn 1.5)

€165.00

View more
BS HR 240:1972

BS HR 240:1972

Superseded Historical

Specification for cobalt-chromium-tungsten-nickel-manganese heat-resisting alloy plate, sheet and strip (cobalt base Cr 20, W 15, Ni 10, Mn 1.5)

€165.00

View more
BS HR 4:1972

BS HR 4:1972

Superseded Historical

Specification for nickel-chromium-cobalt-aluminium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 15, Co 14.2, Al 5, Mo 4, Ti 4)

€165.00

View more
BS HR 3:1972

BS HR 3:1972

Superseded Historical

Specification for nickel-cobalt-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 14.8, Mo 5, Al 4.7, Ti 1.2)

€165.00

View more
BS HR 203:1972

BS HR 203:1972

Superseded Historical

Specification for nickel-chromium-titanium heat-resisting alloy plate, sheet and strip (nickel base, Cr 19.5, Ti 0.4)

€165.00

View more
BS HR 204:1972

BS HR 204:1972

Superseded Historical

Specification for nickel-chromium-iron-molybdenum-cobalt-tungsten heat-resisting alloy plate, sheet and strip (nickel base Cr 22, Fe 18.5, Mo 9, Co 1.5, W 0.6)

€81.00

View more
DIN 52332:1971-04

DIN 52332:1971-04

Withdrawn Most Recent

Testing of glass; determination of the solubility of the binder of glass fibre mats in styrene

€24.39

View more
DIN 52316:1970-10

DIN 52316:1970-10

Withdrawn Most Recent

Testing of glass; determination of stiffness of continuous filament glass fibre rovings

€24.39

View more
BS 3L 124:1970

BS 3L 124:1970

Withdrawn Most Recent

Specification for ingots and castings of magnesium - 10% aluminium-zinc-manganese alloy (solution treated) (Al 10, Zn 0.5, Mn 0.3)

€165.00

View more
BS 3L 125:1970

BS 3L 125:1970

Withdrawn Most Recent

Specification for ingots and castings of magnesium - 10% aluminium-zinc-manganese alloy (solution treated and precipitation treated) (Al 10, Zn 0.5, Mn 0.3)

€165.00

View more
BS 2L 127:1970

BS 2L 127:1970

Withdrawn Most Recent

Specification for ingots and castings of magnesium-zinc-zirconium alloy (precipitation treated) (Zn 4.5, Zr 0.7)

€165.00

View more
ASTM F314-70(1980)

ASTM F314-70(1980)

Withdrawn Most Recent

Methods of Test for Identification of Metallic and Fibrous Contaminants in Aerospace Fluids (Withdrawn 1990)

This product is not for sale, please contact us for more information

View more
BS 2V 37:1968

BS 2V 37:1968

Withdrawn Most Recent

Specification for Sitka spruce as finished timber

€165.00

View more
BS V 38:1967

BS V 38:1967

Withdrawn Most Recent

Specification for Sitka spruce as rough timber

€165.00

View more