Steel Castings, Sand, Corrosion Resistant 16Cr - 1.9Ni (Type 431 Mod) Normalized and Tempered
€90.00
Alloy Castings, Investment, Corrosion and Heat Resistant 65.5Co - 25Cr - 1.8Ni - 5.0W As Cast
ACID, INHIBITED PHOSPHORIC Aircraft Turbine Engine Components Room Temperature Application
€75.00
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1750 °F (954 °C) Solution Heat Treated
€70.00
Standard Test Method for Gravimetric Determination of Nonvolatile Residue from Cleanroom Gloves
This product is not for sale, please contact us for more information
Standard Test Method for Gravimetric Determination of Nonvolatile Residue From Cleanroom Wipers
Magnesium Alloy, Sheet and Plate, 2.0Th - 0.78Mn, Solution Heat Treated, Cold Worked, and Precipitation Heat Treated
€71.00
Magnesium Alloy, Sheet and Plate, 3.2Th - 0.70Zr, Annealed Recrystallized
€81.00
Magnesium Alloy, Sheet and Plate, 3.2Th - 0.70Zr, Cold Rolled and Partially Annealed
€77.00
Magnesium Alloy Castings, Sand, 6.0Al - 3.0Zn (AZ63 - T4), Solution Heat Treated
Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 78Ni - 20Cr
€68.00
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated
Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 62Ni - 21.5Cr - 9.0Mo - 3.7Cb(Nb)
Trace Element Control, Nickel Alloy Castings
€67.00
Powder, Plasma Spray 50 (88WC - 12Co) + 35 (70Ni - 16.5Cr - 4Fe - 4Si - 3.8B) + 15 (80Ni - 20A1) Three-Component Mixture