Standard Test Method for Thermal Endurance of Coating Powders Used for Integral Bus Bar Insulation Systems

Disponibilité: En stock.

61,00 €

Détails

1.1 ,This test method provides a procedure for evaluating thermal endurance of coating powders by determining the length of aging time at selected elevated temperatures required to achieve dielectric breakdown at room temperature at a pre-determined proof voltage. Thermal endurance is expressed in terms of a temperature index.

1.2 ,This test method is applicable to insulating powders used over a substrate material of copper or aluminum.

1.3 ,Units—,The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system are not necessarily exact equivalents, therefore, each system shall be used independently of the other. Combining values from the two systems is likely to result in non-conformance with the standard.

1.4 ,This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in Section 7.

1.5 ,This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.


Significance and Use:

5.1 ,A major factor affecting the life of insulating materials is thermal degradation. It is possible that other factors, such as moisture and vibration, will cause failures after the material has been weakened by thermal degradation.

5.2 ,Electrical insulation is effective in electrical equipment only as long as it retains its physical and electrical integrity. The following are potential indicators of thermal degradation: weight change, porosity, crazing, and generally a reduction in flexibility. Thermal degradation is usually accompanied by an ultimate reduction in dielectric breakdown.

5.3 ,This test method is useful in determining the thermal endurance of coating powders applied over a copper or aluminum substrate material.

Informations supplémentaires

Auteur American Society for Testing and Materials (ASTM International)
Comité D09.01 - Committee D09 on Electrical and Electronic Insulating Materials
Edité par ASTM
Type de document Norme
Thème ,Wires,Insulation in general,Paints and varnishes
ICS 29.060.10 : Fils
29.080.01 : Isolation électrique en général
87.040 : Peintures et vernis
Nombre de pages 6
Remplace ASTM D7894/D7894M-14(2018) + Redline
Recueil ASTM Volume 10.02 - Multi-User - Single-Site Online
Historique ,
Mot-clé D7894/D7894M

Vous pourriez aussi être intéressé(e) par le(s) produit(s) suivant(s)